Goldvault Header Safety placqard
Assay Photos Page   Main Page    Bottom
Crucibles in the furnace. A button from cupel mold Slag and lead cube.
Ore charges being fired at 2000 degrees fahrenheit Charge after cooling in cupel mold. Note division of slag and lead After slag is broken from button, the lead cone is shaped into a cube.
This lead cube contains any precious values. Cupels in the furnace Assay bead 375mg
Lead cube contains any precious values and is ready for cupelling. Cupelling at 1750 degrees removes the lead, leaving any values behind. The assay bead remaining is usually gold combined with silver.
Assay beads highly magnified. Assorted assay slags. Assaying balance readout.
Assay Beads, .1mg to 65mg. Each mg.= 1 troy oz value per ton of ore. Assay slags. Colors reflect the various minerals in the ore. Assay balance showing readout of 8 ten-thousands of 1 gram

Return to Top   Main Page